Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of RADILON ADLINE CS - PA666 - RadiciGroup High Performance Polymers

Material Data Center offers the following functions for RADILON ADLINE CS:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Radilon A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
PA6/66 copolymer for 3D Printing Fused Deposition Modelling.

Suitable for parts requiring high dimensional stability and very reduced shrinkage. Transparent material, it offers good surface aspect and easy processability.
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 2005 / - MPa ISO 527
Yield stress 55 / - MPa ISO 527
Yield strain 4.5 / - % ISO 527
Nominal strain at break 15 / - % ISO 527
Charpy impact strength, +23°C N / - kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 30 / - kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 195 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 45 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 50 / * °C ISO 75-1/-2
Other propertiesdry / condUnitTest Standard
Water absorption 10.2 / * % Sim. to ISO 62
Humidity absorption 3 / * % Sim. to ISO 62
Density 1100 / - kg/m³ ISO 1183
Characteristics
Processing
Additive Manufacturing
Delivery form
Granules
Special Characteristics
Transparent
Features
Copolymer
Regional Availability
Other text information
Injection molding
The material is available in granules or in filament – 1.75 mm and 2.85 mm diameter.
In the case of granules, the material is delivered in moisture-proof packaging ready for processing. Maximum recommended water content for best processing is 0.10%. Typical conditions with a desiccant drier: temperature 80 ° C, dew point -20 ° C or below, time 2-4 h or more. In the case of filaments, the material is originally sealed in vacuum bags with silica gel inside to keep environment in dry conditions. For best printing results, it is recommended to pre-dry the filament at 70-80°C for 2-4 h or more. Alternatively, Radilon® Adline filaments are compatible with Drywise system from Thought3D Ltd. 

Recommended 3D-Print processing parameters:
 
Nozzle Temperature Bed Temperature Adhesion promoter Print Speed
250°-280°C 70-100°C Magigoo glue 30-40 mm/s


Please note: Parameters are dependent on printer used.
Radici tests were performed on a Ultimaker S5 printer
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.